Application: Foaming of Polyolefins and styrenics
during extrusion and injection molding. Fine closed cells and smooth
surface quality.
Active Ingredients: Proprietary multiconponent endothermic
system.
Carrier: LPDE
Active Content: 20 wt. %
Physiology: The raw materials used comply with USFDA
.
Physical Form: White pellets.
Technical Data:
Decomposition Initial: Approximately 150 ° C.
Processing: 190° to 230° C to achieve optimum
gas yields.
Recommended Processing Condition:
Injection Molding: Weight reduction of the molded
part-based on the geometry. 0.3 to 0.7 wt%
Extrusion: Gas assisted chemical foaming. 0.5 to
1 wt %
The above information is offered as true and accurate
to the best of our knowledge. This company makes no guarantee of results