Application: Physical nucleating agent
for polystyrene foam.
Active Ingredients: Proprietary compound.
Carrier: Polystyrene
Active Content:: 50 wt.% Talc
Talc Particle Size: 80% <1 micron. Distribution <1
to 5 microns.
Physical Form: Light brown solid pellets.
Technical Data:
Melting Point Greater than 150°
C.
Processing: 170° to 230° C.
Recommended
Processing Condition:
Foam Extrusion
Fine cell structure of the extruded foam PS using Azo
and /or physical blowing agents.
Use level is 0.4 to 1% by weight of PE
The above information is offered
as true and accurate to the best of our knowledge. This company
makes no guarantee of results and assumes no obligation or liability
in connection with the same.